    Rapid Ref : PTER80SB2-24  

    Lincoln ER80S-B2 Mild Steel TIG Wire, 5Kg Pack
    PTER80SB2-24

    Select Option 
    Prices From £88.80 ex VAT

    1CrMo TIG wire for creep-resisting steels.

    Applications
    These consumables are designed for prolonged elevated temperature service up to 550°C. The main areas of application are associated with a steam-generating power plant, eg piping, turbine castings, steam chests, valve bodies and boiler superheaters. Some of the consumables will also find service in refineries where they are used for corrosion resistance to sulphur-bearing crude oil at 250-450°C. Some of the consumables will also find applications in the chemical and petrochemical industries where they are used for resistance to hydrogen attack in the fabrication of hydrocrackers, coal liquefaction plants and NH3 pressure vessels operating at up to 450°C. In the as-welded condition, the consumables also provide a useful source of 300HV hardness weld deposit for build-up or hard surfacing to resist metal-to-metal wear and heavy impact.

    Specification
    AWS A5.28: ER80S-B2
    BS EN ISO 21952-B: 1CM

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er80S-B2 FAQs

    Answers to common questions about 1.25% chromium, 0.5% molybdenum TIG filler rod for creep-resisting steels.

    What is ER80S-B2 TIG wire used for?icon-minus-redicon-plus-red

    ER80S-B2 is a chromium-molybdenum filler rod with roughly 1.25% chromium and 0.5% molybdenum. It is chosen to weld steels of similar composition that are used at high temperature, such as boiler tube, steam pipework and pressure parts in power and process plant.

    The idea is that the weld metal should match the parent steel's strength and creep resistance at temperature, which an ordinary mild steel rod will not do. Check the drawing, the weld procedure and the parent steel specification to confirm this is the right filler for your job.

    Do I need to preheat when TIG welding with ER80S-B2?icon-minus-redicon-plus-red

    Usually yes. These chromium-molybdenum steels form hard structures that are sensitive to hydrogen cracking, so preheat is normally applied, and the interpass temperature is kept below a set maximum.

    The minimum preheat usually rises with thickness, and the actual figures also depend on restraint and the governing code. Use the preheat and interpass temperatures in your qualified weld procedure, and monitor them with a contact thermometer or temperature-indicating crayons.

    What shielding gas and polarity do I use?icon-minus-redicon-plus-red

    TIG welding of this type of steel is normally done with pure argon shielding and direct current with the torch (tungsten) on negative polarity. This gives a stable arc and a clean, well-shielded weld pool.

    Gas flow rate, tungsten type and size, and current range depend on the joint, the torch and the welder, so set them from your weld procedure and equipment manual. Make sure the gas covers the weld pool and the hot end of the filler rod as you withdraw it, otherwise the rod tip oxidises and the contamination is carried into the next dip.

    Can I use a mild steel TIG rod on chromium-molybdenum steel instead?icon-minus-redicon-plus-red

    For work that has to withstand high temperature, generally no. Welding consumables that match the parent steel's composition are the normal choice, because a plain carbon steel weld would not give the same strength at temperature or the same resistance to creep.

    A different filler may be allowed in some repair or dissimilar joints, but only where the weld procedure and the design code say so. If you are unsure, check with the person responsible for the weld procedure or ask our team to help you identify the right class of rod.