    SIFSteel A32 Steel TIG Wire, 1000mm Cut Lengths - AWS A5.28 ER80S-B2, 5Kg Pack
    RA32XX50

    Select Option 
    Prices From £57.76 ex VAT

    A copper-coated alloy steel rod containing 1.0% chromium, and 0.5% molybdenum. Ideal for creep-resistant steels of similar composition. It is used in the chemical industry and in the ammonia synthesis process, for heat exchangers, boilers, piping and pressure vessels for temperature service up to about 550°c.  It will also find applications in the petro-chemical industries, suitable for facing on casting and for casting repairs.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er80S-B2 FAQs

    Answers to common questions about 1.25% chromium, 0.5% molybdenum TIG filler rod for creep-resisting steels.

    What is ER80S-B2 TIG wire used for?icon-minus-redicon-plus-red

    ER80S-B2 is a chromium-molybdenum filler rod with roughly 1.25% chromium and 0.5% molybdenum. It is chosen to weld steels of similar composition that are used at high temperature, such as boiler tube, steam pipework and pressure parts in power and process plant.

    The idea is that the weld metal should match the parent steel's strength and creep resistance at temperature, which an ordinary mild steel rod will not do. Check the drawing, the weld procedure and the parent steel specification to confirm this is the right filler for your job.

    Which steels does ER80S-B2 match?icon-minus-redicon-plus-red

    It is intended for the 1.25% chromium, 0.5% molybdenum family of creep-resisting steels, often supplied as pipe, tube, plate and forgings. Look at the material certificate or specification of the parent steel and the weld procedure to see which filler is called up.

    For steels with about 2.25% chromium and 1% molybdenum a higher alloyed rod is normally specified instead. If you are joining two different grades, the weld procedure should say which filler to use; do not guess from the rod class alone.

    Is post-weld heat treatment always needed for this wire?icon-minus-redicon-plus-red

    For most creep-resisting steels, post-weld heat treatment (PWHT) is required by the application codes. It softens the hard structures formed in the weld and heat-affected zone and improves toughness.

    The temperature range and soak time depend on the steel, the thickness and the code or specification, and are sometimes adjusted to reach particular properties. Do not pick figures from a rod description. Take them from the weld procedure, and make sure the heating and cooling rates are controlled so the part is not distorted or cracked.

    Can I use a mild steel TIG rod on chromium-molybdenum steel instead?icon-minus-redicon-plus-red

    For work that has to withstand high temperature, generally no. Welding consumables that match the parent steel's composition are the normal choice, because a plain carbon steel weld would not give the same strength at temperature or the same resistance to creep.

    A different filler may be allowed in some repair or dissimilar joints, but only where the weld procedure and the design code say so. If you are unsure, check with the person responsible for the weld procedure or ask our team to help you identify the right class of rod.