ER80S-B2 is a 1.25% Cr/0.5% Mo alloyed wire intended for TIG welding creep-resisting steels of similar composition, used in power generation plant operating at temperatures up to 570°c, e.g. DIN 13 CrMo 44, GS-17 CrMo 55, BS 3604 Grades 620 and 621 etc.  Also suitable for use in the chemical and petrochemical industries where resistance to hydrogen attack, corrosion from sulphur-bearing crude oil and stress corrosion cracking in sour environments is required.   The Mn content fulfils the AWS classification B2.  Preheat and interpass temperature of 150-200°c is recommended.  Post-weld heat treat at 690°c.

  C Si Mn P S Cr Mo
Min 0,08 0,50 0,80     1,10 0,45
Typical 0,11 065 1,00 0,006 0,006 1,20 0,50
Max 0,12 0,70 1,20 0,020 0,020 1,30 0,60

 

Tig Er80S-B2 FAQs

Answers to common questions about 1.25% chromium, 0.5% molybdenum TIG filler rod for creep-resisting steels.

What is ER80S-B2 TIG wire used for?icon-minus-redicon-plus-red

ER80S-B2 is a chromium-molybdenum filler rod with roughly 1.25% chromium and 0.5% molybdenum. It is chosen to weld steels of similar composition that are used at high temperature, such as boiler tube, steam pipework and pressure parts in power and process plant.

The idea is that the weld metal should match the parent steel's strength and creep resistance at temperature, which an ordinary mild steel rod will not do. Check the drawing, the weld procedure and the parent steel specification to confirm this is the right filler for your job.

Which steels does ER80S-B2 match?icon-minus-redicon-plus-red

It is intended for the 1.25% chromium, 0.5% molybdenum family of creep-resisting steels, often supplied as pipe, tube, plate and forgings. Look at the material certificate or specification of the parent steel and the weld procedure to see which filler is called up.

For steels with about 2.25% chromium and 1% molybdenum a higher alloyed rod is normally specified instead. If you are joining two different grades, the weld procedure should say which filler to use; do not guess from the rod class alone.

Do I need to preheat when TIG welding with ER80S-B2?icon-minus-redicon-plus-red

Usually yes. These chromium-molybdenum steels form hard structures that are sensitive to hydrogen cracking, so preheat is normally applied, and the interpass temperature is kept below a set maximum.

The minimum preheat usually rises with thickness, and the actual figures also depend on restraint and the governing code. Use the preheat and interpass temperatures in your qualified weld procedure, and monitor them with a contact thermometer or temperature-indicating crayons.

Is post-weld heat treatment always needed for this wire?icon-minus-redicon-plus-red

For most creep-resisting steels, post-weld heat treatment (PWHT) is required by the application codes. It softens the hard structures formed in the weld and heat-affected zone and improves toughness.

The temperature range and soak time depend on the steel, the thickness and the code or specification, and are sometimes adjusted to reach particular properties. Do not pick figures from a rod description. Take them from the weld procedure, and make sure the heating and cooling rates are controlled so the part is not distorted or cracked.

How do I keep hydrogen out of the weld?icon-minus-redicon-plus-red

Hydrogen is the main cause of cracking in these steels, so low-hydrogen practice matters. TIG is a low-hydrogen process, but only if the joint, filler and gas are clean and dry.

Clean the joint faces and nearby surfaces of oil, paint, grease and moisture before welding. Wipe the rod if it has picked up dirt. Use a high-purity, dry shielding gas and check hoses and fittings for leaks or damp, as moisture in the gas supply can introduce hydrogen. Keep the preheat on until the joint is completed, as the weld procedure requires.

What shielding gas and polarity do I use?icon-minus-redicon-plus-red

TIG welding of this type of steel is normally done with pure argon shielding and direct current with the torch (tungsten) on negative polarity. This gives a stable arc and a clean, well-shielded weld pool.

Gas flow rate, tungsten type and size, and current range depend on the joint, the torch and the welder, so set them from your weld procedure and equipment manual. Make sure the gas covers the weld pool and the hot end of the filler rod as you withdraw it, otherwise the rod tip oxidises and the contamination is carried into the next dip.

Can I use a mild steel TIG rod on chromium-molybdenum steel instead?icon-minus-redicon-plus-red

For work that has to withstand high temperature, generally no. Welding consumables that match the parent steel's composition are the normal choice, because a plain carbon steel weld would not give the same strength at temperature or the same resistance to creep.

A different filler may be allowed in some repair or dissimilar joints, but only where the weld procedure and the design code say so. If you are unsure, check with the person responsible for the weld procedure or ask our team to help you identify the right class of rod.