    Lincoln LNT 19 Steel Tig Wire, 2.4mm Diameter x 1000mm Cut Lengths - AWS A5.28 ER80S-B2. 5.0kg Pack
    604368

    £55.44  EX VAT
    SSP Suggested Selling Price = £69.30  YOU SAVE £13.86
     Buy in 3 easy interest free payments of £18.48† with

    Solid rod for welding creep and hydrogen-resistant Cr-Mo steels (1,25Cr - 0,5Mo). Service temperature up to 550°c.

    Classification
    AWS A5.28 - ER80S-B2 (Nearest classification)
    ISO 21952-A - W CrMo1Si

    Shielding Gas
    l1 Inert gas AR (100%)

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er80S-B2 FAQs

    Answers to common questions about 1.25% chromium, 0.5% molybdenum TIG filler rod for creep-resisting steels.

    Do I need to preheat when TIG welding with ER80S-B2?icon-minus-redicon-plus-red

    Usually yes. These chromium-molybdenum steels form hard structures that are sensitive to hydrogen cracking, so preheat is normally applied, and the interpass temperature is kept below a set maximum.

    The minimum preheat usually rises with thickness, and the actual figures also depend on restraint and the governing code. Use the preheat and interpass temperatures in your qualified weld procedure, and monitor them with a contact thermometer or temperature-indicating crayons.

    Is post-weld heat treatment always needed for this wire?icon-minus-redicon-plus-red

    For most creep-resisting steels, post-weld heat treatment (PWHT) is required by the application codes. It softens the hard structures formed in the weld and heat-affected zone and improves toughness.

    The temperature range and soak time depend on the steel, the thickness and the code or specification, and are sometimes adjusted to reach particular properties. Do not pick figures from a rod description. Take them from the weld procedure, and make sure the heating and cooling rates are controlled so the part is not distorted or cracked.

    How do I keep hydrogen out of the weld?icon-minus-redicon-plus-red

    Hydrogen is the main cause of cracking in these steels, so low-hydrogen practice matters. TIG is a low-hydrogen process, but only if the joint, filler and gas are clean and dry.

    Clean the joint faces and nearby surfaces of oil, paint, grease and moisture before welding. Wipe the rod if it has picked up dirt. Use a high-purity, dry shielding gas and check hoses and fittings for leaks or damp, as moisture in the gas supply can introduce hydrogen. Keep the preheat on until the joint is completed, as the weld procedure requires.

    What shielding gas and polarity do I use?icon-minus-redicon-plus-red

    TIG welding of this type of steel is normally done with pure argon shielding and direct current with the torch (tungsten) on negative polarity. This gives a stable arc and a clean, well-shielded weld pool.

    Gas flow rate, tungsten type and size, and current range depend on the joint, the torch and the welder, so set them from your weld procedure and equipment manual. Make sure the gas covers the weld pool and the hot end of the filler rod as you withdraw it, otherwise the rod tip oxidises and the contamination is carried into the next dip.