Tig Er80S-B2 FAQs
Answers to common questions about 1.25% chromium, 0.5% molybdenum TIG filler rod for creep-resisting steels.
What is ER80S-B2 TIG wire used for?

ER80S-B2 is a chromium-molybdenum filler rod with roughly 1.25% chromium and 0.5% molybdenum. It is chosen to weld steels of similar composition that are used at high temperature, such as boiler tube, steam pipework and pressure parts in power and process plant.
The idea is that the weld metal should match the parent steel's strength and creep resistance at temperature, which an ordinary mild steel rod will not do. Check the drawing, the weld procedure and the parent steel specification to confirm this is the right filler for your job.
Is post-weld heat treatment always needed for this wire?

For most creep-resisting steels, post-weld heat treatment (PWHT) is required by the application codes. It softens the hard structures formed in the weld and heat-affected zone and improves toughness.
The temperature range and soak time depend on the steel, the thickness and the code or specification, and are sometimes adjusted to reach particular properties. Do not pick figures from a rod description. Take them from the weld procedure, and make sure the heating and cooling rates are controlled so the part is not distorted or cracked.
How do I keep hydrogen out of the weld?

Hydrogen is the main cause of cracking in these steels, so low-hydrogen practice matters. TIG is a low-hydrogen process, but only if the joint, filler and gas are clean and dry.
Clean the joint faces and nearby surfaces of oil, paint, grease and moisture before welding. Wipe the rod if it has picked up dirt. Use a high-purity, dry shielding gas and check hoses and fittings for leaks or damp, as moisture in the gas supply can introduce hydrogen. Keep the preheat on until the joint is completed, as the weld procedure requires.
What shielding gas and polarity do I use?

TIG welding of this type of steel is normally done with pure argon shielding and direct current with the torch (tungsten) on negative polarity. This gives a stable arc and a clean, well-shielded weld pool.
Gas flow rate, tungsten type and size, and current range depend on the joint, the torch and the welder, so set them from your weld procedure and equipment manual. Make sure the gas covers the weld pool and the hot end of the filler rod as you withdraw it, otherwise the rod tip oxidises and the contamination is carried into the next dip.