    Rapid Ref : 131624R150  

    ESAB OK Tigrod 13.16 2.4mm TIG Wire, 5Kg Pack. ER80S-B2
    131624R150

    £120.04  EX VAT
    SSP Suggested Selling Price = £130.68  YOU SAVE £10.64
     Buy in 3 easy interest free payments of £40.01† with

    OK Tigrod 13.16 is a 1.3Cr-0.5Mo-alloyed (ER80S-B2), copper-coated rod for the GTAW of creep-resistant steels like SA-387 Grade 11, A 335 Grade P11 or similar materials.  The rod has a high purity chemistry with a guaranteed Bruscato factor X < 15.

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Tig Er80S-B2 FAQs

    Answers to common questions about 1.25% chromium, 0.5% molybdenum TIG filler rod for creep-resisting steels.

    Do I need to preheat when TIG welding with ER80S-B2?icon-minus-redicon-plus-red

    Usually yes. These chromium-molybdenum steels form hard structures that are sensitive to hydrogen cracking, so preheat is normally applied, and the interpass temperature is kept below a set maximum.

    The minimum preheat usually rises with thickness, and the actual figures also depend on restraint and the governing code. Use the preheat and interpass temperatures in your qualified weld procedure, and monitor them with a contact thermometer or temperature-indicating crayons.

    Is post-weld heat treatment always needed for this wire?icon-minus-redicon-plus-red

    For most creep-resisting steels, post-weld heat treatment (PWHT) is required by the application codes. It softens the hard structures formed in the weld and heat-affected zone and improves toughness.

    The temperature range and soak time depend on the steel, the thickness and the code or specification, and are sometimes adjusted to reach particular properties. Do not pick figures from a rod description. Take them from the weld procedure, and make sure the heating and cooling rates are controlled so the part is not distorted or cracked.

    What shielding gas and polarity do I use?icon-minus-redicon-plus-red

    TIG welding of this type of steel is normally done with pure argon shielding and direct current with the torch (tungsten) on negative polarity. This gives a stable arc and a clean, well-shielded weld pool.

    Gas flow rate, tungsten type and size, and current range depend on the joint, the torch and the welder, so set them from your weld procedure and equipment manual. Make sure the gas covers the weld pool and the hot end of the filler rod as you withdraw it, otherwise the rod tip oxidises and the contamination is carried into the next dip.

    Can I use a mild steel TIG rod on chromium-molybdenum steel instead?icon-minus-redicon-plus-red

    For work that has to withstand high temperature, generally no. Welding consumables that match the parent steel's composition are the normal choice, because a plain carbon steel weld would not give the same strength at temperature or the same resistance to creep.

    A different filler may be allowed in some repair or dissimilar joints, but only where the weld procedure and the design code say so. If you are unsure, check with the person responsible for the weld procedure or ask our team to help you identify the right class of rod.